Shrink Sleeve Lay Flat Formula: From Bottle to Order Spec
The shrink sleeve lay flat formula worked step by step: diameter conversion, the shrink a lay-flat demands, cut length, unfolded width and a worked bottle example.
Lay-flat width is the width of a seamed shrink sleeve pressed flat, measured fold to fold, so it equals half the sleeve’s circumference. The common shrink sleeve lay flat formula is the container’s widest circumference ÷ 2 + about 3 mm.
Key takeaways
- From a diameter, lay-flat = 1.571 × D + 3 mm; any lay-flat converts back to the opened tube’s diameter as 0.637 × lay-flat.
- Required transverse (TD) shrink = 1 − narrowest grip circumference ÷ (2 × lay-flat), with the clearance allowance already built in.
The shrink sleeve lay flat formula
Lay-flat = widest circumference ÷ 2 + about 3 mm.
Neck and tamper bands are sized on the same principle with a slightly smaller allowance, as the tamper-evident shrink band guide explains.
How to measure lay-flat width: the bottle and the finished sleeve
A sleeve already in use, or a length drawn off a roll of seamed tubing, gives the shrink sleeve layflat directly, read with calipers between the two folded edges without stretching.
| Measurement | How it is taken | Used for |
|---|---|---|
| Widest circumference | Tape around the fattest section, counting flanges, flares and any cap the sleeve covers | Lay-flat |
| Narrowest grip circumference | Tape at the tightest point the sleeve must hug: waist, neck or shoulder | Required TD |
| Contour length | Tape laid along the surface from the sleeve’s top edge to its bottom edge | Cut length |
Lay flat width to diameter, and diameter to lay flat
Lay-flat and diameter convert with two fixed factors, lay-flat = 1.571 × diameter and diameter = 0.637 × lay-flat, because a sleeve’s circumference is at once 2 × lay-flat and π × diameter.
Cut length and unfolded width: the other two sleeve dimensions
Cut length is the coverage length measured along the contour, divided by (1 − MD) to put back the strip that machine-direction shrink will take out, while the unfolded width is roughly 2 × lay-flat + 7–8 mm of flat film per sleeve before seaming.
How to calculate shrink sleeve size: a worked example
Tape readings are to the nearest millimetre and the cut length assumes MD = 3.0%.
Example: waisted bottle. This contour matches the deep-waisted bottle in the shrink rate guide: a 76 mm shoulder and a 34 mm waist, which tape at 239 mm and 107 mm, over 180 mm of contour. Here 239 ÷ 2 + 3 = 122.5, rounded up to a 123 mm lay-flat and a 246 mm sleeve. At the waist, 1 − 107 ÷ 246 ≈ 57%. Cut length comes to 180 ÷ 0.97 = 185.6 mm and unfolded width to 253–254 mm.
Too much overlap or the wrong lay-flat: what each one causes
A lay-flat that is too small cannot pass the widest point and jams on the applicator. One that is too large raises the shrink the film has to deliver at the narrow point, and seam overlap beyond what the bond needs only adds a band of double film.
Wrinkles and loose areas can also come from tunnel temperature and airflow, so checking the lay-flat is only one step in tracing them.
The numbers to put on a shrink sleeve spec
A supplier can quote a sleeve from four numbers — lay-flat, cut length, required TD and thickness — while the unfolded width per sleeve is the starting point for the film width.
- Lay-flat width (mm): half the widest circumference plus the allowance, checked against the applicator’s requirement on automatic lines.
- Cut length (mm): contour length ÷ (1 − MD), using the MD of the film actually being ordered.
- Required TD (%): calculated at the narrowest grip point, with the film’s rated shrink chosen above it.
- Thickness (μm): chosen for the container and the line, as set out in the shrink film thickness guide.
- Unfolded width (mm): 2 × lay-flat + 7–8 mm, the basis for the film width; roll length and diameter are a separate roll length calculation.
Our clear PETG shrink film is supplied at TD ≥75%, MD ≤3.0%, 30–60 μm thick and 200–2000 mm wide; the TD and MD figures are the film values these formulas use.
Frequently Asked Questions
Is there a standard shrink sleeve size chart?
Why is there excess film or extra wrapping on a PETG sleeve?
Does the lay-flat formula depend on the film material?
Related Articles
How Is PETG Shrink Film Made? Where Roll Quality Is Decided
How PETG shrink film is made, and which production stage sets each line buyers check on arrival: gauge tolerance, TD/MD shrink, haze, tensile strength, roll labels.
Shrink Film Roll Length Calculation: The 3-Inch Core Trap
The formula linking roll diameter, core, thickness and length, a worked example with the imperial constant, and why core size and trapped air shift the result.
Need Expert Advice on Shrink Film?
Our technical team can help you choose the right film for your application.
Contact Us